Items where Year is 2011
Number of items at this level: 46. AAbang Mahmod, Dayang Salyani (2011) Preparation and characterization of polyacrylonitrile fiber precusor using multi-hole spinneret. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. Abd. Rahim, Nurul Hanan (2011) Fabrication and characterization of polyethersulfone multi-walled carbon nanotubes mixed matrix membranes for gas separation. PhD thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. Abu Bakar, Kamarudin and Rajiani, Ismi and Ayob, Md. Razali and Nasri, Noor Shawal (2011) Fostering green strategy through "a-f-f-i-r-m" model for sustainable development within the environmental-socio-economic system in Malaysia. In: International Conference On Management (ICM 2011) Proceeding. Ahmad Kueh Beng Hong (2011) Size dependent uniaxially loaded stability of triaxial weave fabric composites. In: 2011 International Conference On Civil Engineering And Transportation (ICCET 2011). Akhondzadeh, Hamed (2011) Eor by expanding solvent steam assisted gravity drainage in athabasca oil reservoir. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. BBruun, Esben Wilson and Hauggaard-Nielsen, Henrik and Ibrahim, Norazana and Egsgaard, Helge and Ambus, Per Lennart and Jensen, Peter Arendt and Kim, Dam-Johansen (2011) Influence of fast pyrolysis temperature on biochar labile fraction and short-term carbon loss in a loamy soil. Biomass and Bioenergy, 35 (3). pp. 1182-1189. ISSN 0961-9534 GGoh, Pei Sean and Ismail, A. F. and Sanip, S. M. and Ng, B. C. and Aziz, M. (2011) Recent advances of inorganic fillers in mixed matrix membrane for gas separation separation. Separation and Purification Technology, 81 . pp. 243-264. ISSN 1383-5866 HHamid, N. A. A. and Ismail, Ahmad Fauzi and Matsuura, T. and Zularisam, A. W. and Lau, W .J. and Yuliwati, Er and Abdullah, Mohd. Sohaimi (2011) Morphological and separation performance study of polysulfone/ titanium dioxide (PSF/ TIO2) ultrafiltration membranes for humic acid removal. Desalination, 273 . pp. 85-92. ISSN 0011-9164 Hasbullah, H. and Kumbharkar, S. and Ismail, Ahmad Fauzi and Li, K. (2011) Preparation of polyaniline asymmetric hollow fiber membranes and investigation towards gas separation performance. Journal of Membrane Science, 366 (1-2). pp. 116-124. ISSN 0376-7388 Hashemifard, S. A. and Ismail, A. F. and Matsuura, T. (2011) Effects of montmorillonite no-clay fillers on PEI mixed matrix membrane for CO2 removal. Chemical Engineering Journal, 170 (1). pp. 316-325. ISSN 1385-8947 Hashemifard, S. A. and Ismail, Ahmad Fauzi and Matsuura, Takeshi (2011) Mixed matrix membrane incorporated with large pore size halloysite nanotubes (HNT) as filler for gas separation: experimental. Journal of Colloid and Interface Science, 359 (2). pp. 359-370. ISSN 0021-9797 Hashemifard, S. A. and Ismail, Ahmad Fauzi and Matsuura, Takeshi (2011) Mixed matrix membrane incorporated with large pore size halloysite nanotubes (HNTs) as filler for gas separation: morphological diagram. Chemical Engineering Journal, 172 . pp. 581-590. ISSN 1385-8947 IIdroas, Mariani and Ibrahim, M. Nasir and Khamis, Aishah (2011) Imaging particle profile in liquid flow using optical tomography based on high resolution linear image sensor. In: Progress in Process Tomography & Instrumentation System: Series 3/ 2011. Penerbit UTM Press, Skudai, Johor, pp. 89-103. ISBN 978-967-354-180-5 Idroas, Mariani and Mahmudin, Ahmad Syahril and Ibrahim, M. Nasir and Ramli, Norhafizah and A. Ghani, M. Amir Hamzah (2011) The effect of light time constant of the pulsing system in CCD-based optical tomography. In: Progress in Process Tomography & Instrumentation System: Series 6. Penerbit UTM Press, Skudai, Johor, pp. 253-265. ISBN 978-967-354-184-3 Idroas, Mariani and Sapi’ee, Nora Faaria and Ibrahim, M. Nasir and Md. Zin, A. Ridhwan and M. Najib, Suhaila (2011) A comparison between linear backprojection (transpose) and layergram backprojection methods for image reconstruciton in charged- couple device (CCD) based optical tomography. Jurnal Teknologi (Sciences and Engineering), 55 (2). pp. 23-31. ISSN 0127-9696 Ismail, A. S. I. and Ismail, I. and Peng, Buah W. A. P. and Piroozian, A. (2011) The effect of matrix acidizing on the compressive strength of sandstone formation. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 175-191. ISSN 0127-9696 Ismail, Ahmad Fauzi and Hashemifard, S. A. and Matsuura, T. (2011) Facilitated transport effect of ag+ ion exchanged halloysite notubes on the performance of polyetherimide mixed matrix membrane for gas separation. Journal of Membrane Science, 379 . pp. 378-385. ISSN 0376-7388 Ismail, Ahmad Fauzi and Rahim, N. H. and Mustafa, A. and Matsuura, Takeshi and Ng, B. C. and Abdullah, Mohd. Sohaimi and Hashemifard, S. A. (2011) Gas separation performance of polyethersulfone/multi-walled carbon nanotubes mixed matrix membranes. Separation and Purification Technology, 80 (1). pp. 20-31. ISSN 1383-5866 Ismail, Ahmad Fauzi and Ridzuan, Norida and Wan Abdul Rahman, Wan Aizan and Matsuura, T. and Hashemifard, S. A. (2011) Preparation and characterization of hyperthin-skinned and high performances asymmetric polyethersulfone membrane for gas separation. Desalination, 273 (1). pp. 93-104. ISSN 0011-9164 Ismail, I. and Azizi, Che Yunus M. and Ismail, A. S. and Ibrahim, A. A. (2011) The use of lignosulfote from empty fruit bunches as corrosion inhibitor. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 101-112. ISSN 0127-9696 Ismail, I. and Kamis, A. and Mamat, N. S. (2011) Reducing friction during drilling in water-based mud using glass beads. Jurnal Teknologi, 55 . pp. 39-52. ISSN 0127-9696 JJaafar, Juha and Ismail, Ahmad Fauzi and Matsuura, T. and Gai, K. (2011) Performance of speek based polymer-noclay inorganic membrane for DMFC. Journal of Membrane Science, 382 . pp. 202-211. ISSN 0376-7388 Jaafar, Mohd Zaidi and Pourbasirat, Ali (2011) Measurement of streaming potential coupling coefficient on carbote rocks for downhole monitoring in smart wells. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 87-99. ISSN 0127-9696 Junin, Radzuan and Amirian, Tahmineh and Idris, Ahmad Kamal (2011) Adsorption of nanonionic surfactants on clay minerals. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 113-122. ISSN 0127-9696 KKasmani, R. M. and Andrews, G. E. and Phylaktou, H. N. (2011) The influence of vessel volume and equivalence ratio in vented gas explosions. Jurnal Teknologi, 56 (1). pp. 155-164. ISSN 0127–9696 LLau, Woei Jye (2011) Progress in interfacial polymerization technique on composite membrane preparation. In: The 2011 2nd International Conference On Environmental Engineering And Applications (Iceea 2011). MMajid, Z. A. and Mohsin, R. and Yusof, M. Z. (2011) Experimental and computational failure analysis of natural gas pipe. Engineering Failure Analysis, 19 . pp. 32-42. ISSN 1350-6307 Mansourizadeh, Amir (2011) Co2 absorption by mea through porous pvdf hollow fiber membrane. In: Regional Symposium And Workshop On Membrane Science And Technology 2011 (Mst 2011). Mansourizadeh, Amir (2011) Fabrication and characterization of polymeric hollow fiber membranes with nano-scale pore sizes. In: The International Conference For Nanomaterials Synthesis And Characterization (Insc 2011). Mansourizadeh, Amir (2011) Nano-scale pore size asymmetric hollow fiber membranes for carbon dioxide capture. In: International Conference On Nanotechnology Research And Commercialisation (Icont 2011). Mansourizadeh, Amir and Ismail, Ahmad Fauzi (2011) CO2 stripping from water through porous PVDF follow fiber membrane contactor. Desalination, 273 . pp. 386-390. ISSN 0011-9164 Mansourizadeh, Amir and Ismail, Ahmad Fauzi (2011) CO2 stripping from water through porous PVDF hollow fiber membrane contactor. Desalination, 273 (2-3). pp. 386-390. ISSN 0011-9164 Mansourizadeh, Amir and Ismail, Ahmad Fauzi (2011) A developed asymmetric PVDF hollow fiber membrane structure for CO2 absorption. International Journal of Greenhouse Gas Control, 5 (2). pp. 374-380. ISSN 1750-5836 Mohammadain, Erfan and Shirazi, Mohammad Amin and Parak, Mahdi and Idris, Ahmad Kamal and Junin, Radzuan (2011) Improved oil recovery by application of ultrasonic stimulated waterflooding. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 123-138. ISSN 0127-9696 (Print); 2180-3722 (Online) Mohd. Sanip, Suhaila and Ismail, Ahmad Fauzi and Goh, Pei Sean and Soga, T. and Tanemura, M. and Yasuhiko, H. (2011) Gas separation properties of functionalized carbon nanotubes mixed matrix membranes. Separation and Purification Technology, 78 . pp. 208-213. ISSN 1383-5866 Mohtar, S. S. and Ismail, Ahmad Fauzi and Matsuura, Takeshi (2011) Preparation and characterization of speek/ mmt-sta composite membrane for DMFC application. Journal of Membrane Science, 371 . pp. 10-19. ISSN 0376-7388 Mohtar, Safia Syazana (2011) Proton conducting composite membrane based on sulfonated poly (ether ether ketone) silicotungstic acid-montmorillonite. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. PParak, Mahdi (2011) The effects of mixed surfactant on adsorption in different clay minerals. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. Pourbasirat, Ali (2011) Measurement of streaming potential coupling coefficent of carbonate core for downhole monitoring in smart wells. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. SSahir, Zalilah Sharer and Sykes, John Malcolm (2011) Investigation of blister formed on coated mild steel using scanning Kelvin Probe. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 139-154. ISSN 0127-9696 Souhaimi, M. K. and Ismail, A. F. (2011) Special issue honoring Takeshi Matsuura. Desalination . ISSN 0011-9164 WWan Sulaiman, W. Z. and Kasmani, C. R. M. (2011) An overview of explosion severity on dust explosion. Jurnal Teknologi (Sciences and Engineering), 56 (1). pp. 165-174. ISSN 0127-9696 YYuliwati, Erna and Ismail, Ahmad Fauzi and Matsuura, Takeshi and Kassim, Mohd. Azraai and Abdullah, Mohd. Sohaimi (2011) Characterization of surface-modified porous PVDF hollow fibers for refinery wastewater treatment using microscopic observation. Desalination, 283 . pp. 206-213. ISSN 0011-9164 ZZahoor, Muhammad Khurram (2011) Predicting effects of wettability variations on displacement behavior and their incorporation into inflow performance. Masters thesis, Universiti Teknologi Malaysia, Faculty of Petroleum and Renewable Energy Engineering. Zoveidavianpoor, Mansoor and Samsuri, Ariffin and Shadizadeh, Seyed Reza (2011) The needs for hydraulic fracturing in Iranian carbonate oilfields: acid or propped fracture? In: The First National Conference Of Novel Technologies In Oil & Gas Industries. Zularisam, A. W. and Ahmad, A. and Sakih, M. and Ismail, A. F. and Matsuura, T. (2011) Role of rural organic matter (NOM), colloidal particles and solution chemistry on ultrafiltration performance. Separation and Purification Technology, 78 . pp. 189-200. ISSN 1383-5866 |