Khoo, S. J. and Johar, M. and Low, K. O. and Wong, K. J. (2017) Interfacial shear strength characterisation of alkali treated bamboo bundle\x96polyester composites using an improved technique. Plastics, Rubber and Composites, 46 (10). pp. 450-457. ISSN 1465-8011
Full text not available from this repository.
Official URL: https://www.scopus.com/inward/record.uri?eid=2-s2....
Abstract
This study examined the influences of alkali concentration on the interfacial characteristics of bamboo–polyester. Pull-out tests were carried out using a newly designed jig to minimise the fibre breakage during clamping. Bamboo bundles were embedded at 3, 5, 7 and 10 mm and alkali concentrations ranged from 0, 1, 3, 5 to 7 wt-%. The attenuated total reflectance-Fourier transform infrared spectroscopy spectra revealed hemicelluloses was observed at ∼1030 cm−1. The pull-out results showed that interfacial characteristics were not influenced by the embedded length. Furthermore, the highest apparent interfacial shear strength was attained at 3 wt-% concentration, with approximately three times higher compared to the untreated one. A comparison with data from the literature showed that both untreated and treated bamboo/polyester composites have the weakest interfacial bonding. Scanning electron micrographs revealed that alkali treatment has resulted in interface enhancement through chemical modification, mechanical interlocking and frictional contact.
Item Type: | Article |
---|---|
Uncontrolled Keywords: | alkali treatment, Bamboo bundle, interfacial shear strength, polyester, pull-out, scanning electron micrographs |
Subjects: | T Technology > TJ Mechanical engineering and machinery |
Divisions: | Mechanical Engineering |
ID Code: | 77043 |
Deposited By: | Fazli Masari |
Deposited On: | 30 Apr 2018 14:36 |
Last Modified: | 30 Apr 2018 14:36 |
Repository Staff Only: item control page